详细介绍:
35WW250, 35WW300, 35WW270。 35WW400, 35WW440, 50WW290, 50WW310, 50WW350, 50WW400, 50WW440, 50WW470, 50WW600, 50WW800,50WW1000, 50WW1300 35W300 35W330 35W360 35W400,35W440,35W550, 50W310,50W330,50W350,50W400,50W470,50W540,50W600,50W700,50W800....硅钢片、硅钢板、电工钢板、电工钢卷
销售热线:0769-83067889,15820808718 曹静
★宝钢高效能硅钢片:B35AH300,B35A300,B35A250,B35A230,B35A270,B35A440,B50AH300、B50A270,B50A250,B50A300,B50A350,B50A400,50AH470、50AH600、50AH800、B50AH470、B50AH600、B50AH800、B50AR300 B20AT1500
★冷连轧碳素钢板及钢带牌号:SPCC,SPCD,拉伸铁板SPCE深冲压钢板SPCEN,JSC270C镀锌卷/无花镀锌板,JSC270D冷连轧低碳钢板,JSC270E,JSC270F,JSC260G
★冷连轧低碳钢板及钢带牌号:DC01,DC03,DC04,DC05冷连轧低碳钢板,DC06,ST12,ST13德国进口镀锌板 ,ST14,ST15,ST16
★冲压用冷连轧钢板及钢带:BLC,BLD,BUSD,BUFD,BSUFD,FeP01,FeP03,FeP04,FeP05,FeP06
★冷连轧碳素结构钢板:St37-2G,St44-3G,St52-3G
★加磷高强度冷轧钢板及钢带:B170P1,B210P1,B250P1,B180P2,B220P2,BP340,BP380
★烘烤硬化高强度冷轧钢板:B140H1,B180H1,B180H2,
★双相高强度冷轧钢板:B240/390DP,B280/440DP,B340/590DP,B400/780DP
★硅钢铁损值
硅钢片在某一特定频率的交流磁场下,磁化到特定的磁通密度时,每单位重量之硅钢片所损失的能量,称为铁损值。通常所用的交流磁场频率为50或60赫兹,而所达到的磁通密度通常为1.5或1.7特斯拉。常用的铁损值单位是每公斤或每磅硅钢片所损失的瓦特值,用Watt/kg或Watt/lb表示。硅钢片的铁损值来源包括磁滞损、涡电流损和异常涡电流损三部份。硅钢片在磁化的过程中,会产生磁滞的现象。磁滞损即为B-H磁滞曲线所包涵的面积。硅钢片的涡电流损起源于在交流变化的磁场,因法拉第定理的影响,硅钢片内部产生诱导电压,依照奥姆定律,电压在硅钢片内部引起诱导电流,进而造成硅钢片的焦耳热,这项能源损失称为涡电流损。根据古典电磁学理论,涡电流损和钢片的厚度、电阻系数、磁通密度和频率有关。而涡电流损和钢片厚度的平方成正比,和钢片的电阻系数成反比,因此,高级的硅钢片,其厚度倾向较薄,而为了提高钢片的电阻系数,则在硅钢片中添加硅、铝等元素。铁损值减去磁滞损和涡电流损后的能源损失,称为异常涡电流损。学者认为异常涡电流损是由于磁域移动和转动所引起的微观涡电流损失,因此,异常涡电流损和磁域大小有关。若硅钢片的磁域大,当磁化时,其旋转较快,微观涡电流损失增加。铁损值是硅钢片最重要的性质指标,也是各种工业标准对硅钢片分级的规格依据。铁损值愈低,表示品级愈高,其能源效率愈高。
|